Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
5 seconds; ASTM D2240
Tensile Strength, Yield 2.93 MPa
425 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.000827 GPa
0.120 ksi
ASTM D412
Tear Strength 10.5 kN/m
60.0 pli
ASTM D624
Compression Set 13 %
13 %
23°C, 22 hr.; ASTM D395, Method B
24 %
24 %
70°C, 22 hr.; ASTM D395, Method B
44 %
44 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746