Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
5 seconds; ASTM D2240
50
50
Instantaneous; ASTM D2240
Tensile Strength, Yield 3.62 MPa
525 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
100% Modulus 0.00152 GPa
0.220 ksi
ASTM D412
Tear Strength 14.5 kN/m
83.0 pli
ASTM D624
Compression Set 16 %
16 %
23°C, 22 hr.; ASTM D395, Method B
32 %
32 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746