Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ter Hell Plastic Terez® PA 6.6 7510 GF 50 Polyamide 66, 50% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Ter Hell Plastic GMBH
Trade Name Terez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ter Hell Plastic Terez® PA 6.6 7510 GF 50 Polyamide 66, 50% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PA66 with medium viscosity, 50% glass fiber reinforced.Application: For molding parts with very high stiffness at good thermal stability.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
ISO 1183
Water Absorption 4.0 %
4.0 %
ISO 62
Moisture Absorption at Equilibrium 1.4 %
1.4 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 190 MPa
27600 psi
dry; ISO 527
Tensile Strength, Yield 195 MPa
28300 psi
dry; ISO 527
Elongation at Break 1.5 %
1.5 %
dry; ISO 527
Elongation at Yield 1.0 %
1.0 %
dry; ISO 527
Tensile Modulus 15.9 GPa
2310 ksi
dry; ISO 527
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 500 V
500 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 270 - 290 °C
518 - 554 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour