Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

The Chemical Company Nature-Flexx 509 Acetyl Tributyl Citrate, C20H34O8

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer The Chemical Company
Trade Name Nature-Flexx
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF The Chemical Company Nature-Flexx 509 Acetyl Tributyl Citrate, C20H34O8.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NatureFlexx 509 plasticizer or Acetyl Tri-n-Butyl Citrate (ATBC), a tributyl ester, is an innocuous plasticizer of PVC, cellulose resin and synthetic rubber. The chemical compound is used to fulfill plastic industry needs for non-toxic plasticizers that provide flexibility in soft toys for children, medical products such as blood bags, food packaging materials, and cosmetics.The liquid chemical is a colorless organic compound belonging to the carboxylic acid family. It exists in all plants, particularly lemons and limes as well as in many animal tissues and fluids.Molecular Formula: C20H34O8Information provided by The Chemical Company
Physical Properties Metric English Comments
Specific Gravity 1.045 - 1.055 g/cc
1.045 - 1.055 g/cc
(25/25°C)
Optical Properties Metric English Comments
Refractive Index 1.441 - 1.4425
1.441 - 1.4425
(25°C/D)
Component Elements Properties Metric English Comments
Arsenic, As <= 0.00030 %
<= 0.00030 %
Lead, Pb <= 0.0010 %
<= 0.0010 %
Heavy metal content
Chemical Properties Metric English Comments
Acid Value <= 0.20
<= 0.20
mg KOH/gm
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
Weight percent
Descriptive Properties Value Comments
Appearance Colorless Transparent Liquid
Assay = 99.0%
Hazen Color Value (pt-co) = 30
Users viewing this material also viewed the following: