Material Notes:
Synthetic FiberEPDM BinderModerate Caustics and AcidsGood Oil Swell CharacteristicsExcellent Aging PropertiesGood in Light Duty SteamInformation provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM F1315
Thickness 1588 microns
62.52 mil
Thickness tested
Electrical Properties Metric English Comments
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149-95a
Descriptive Properties Value Comments
Color White/Grey
(Top/Bottom)
Compressibility 7 percent
ASTM F36J
Creep Relaxation 25 percent
1/32", ASTM F38B
Gas Permeability <0.5 ml/min
DIN 3535/6
Klinger Hot Compression Test 5 percent
Additional, Thickness Decrease 572°F (300°C), tested at 3,625-psi gasket stress
9 percent
Initial, Thickness Decrease 73°F (23°C), tested at 3,625-psi gasket stress
Leachable Chloride Content 200 ppm
FSA Method (Typical)
Recovery >50 percent
ASTM F36J
Sealability <0.3 ml/hr
1/32", ASTM F37A
Thickness Increase 0-15%
ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
0-20%
ASTM Fuel A, 5h/73°F (23°C)
15-30%
ASTM Oil IRM903, 5h/300°F (149°C)
5-20%
ASTM Fuel B, 5h/73°F (23°C)
Weight Increase <25%
ASTM F146 after immersion in Fuel B 5h/73°F (23°C)