ThyssenKrupp SECURE 500 Structural Steel

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer ThyssenKrupp
Trade Name SECURE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ThyssenKrupp SECURE 500 Structural Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 500 for civil use, that is usually produced in thickness from 3 mm up to 90 mm.Application: The steels may be used for purposes of ballistic protection mainly for applications like armoured limousines and valuable transporters.Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 1600 MPa
232000 psi
Tensile Strength, Yield 1300 MPa
189000 psi
Elongation at Break 9.0 %
9.0 %
Charpy Impact 15.0 J

@Temperature -40.0 °C
11.1 ft-lb

@Temperature -40.0 °F
Transverse
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.050 %

@Thickness >=50.0 mm
<= 0.050 %

@Thickness >=1.97 in
<= 0.11 %

@Thickness 50.0 mm
<= 0.11 %

@Thickness 1.97 in
Carbon, C <= 0.32 %
<= 0.32 %
Chromium, Cr <= 1.5 %
<= 1.5 %
Manganese, Mn <= 0.50 %

@Thickness >=50.0 mm
<= 0.50 %

@Thickness >=1.97 in
<= 1.0 %

@Thickness 50.0 mm
<= 1.0 %

@Thickness 1.97 in
Molybdenum, Mo <= 0.50 %

@Thickness 50.0 mm
<= 0.50 %

@Thickness 1.97 in
<= 0.60 %

@Thickness >=50.0 mm
<= 0.60 %

@Thickness >=1.97 in
Nickel, Ni <= 0.70 %

@Thickness 50.0 mm
<= 0.70 %

@Thickness 1.97 in
<= 3.7 %

@Thickness >=50.0 mm
<= 3.7 %

@Thickness >=1.97 in
Phosphorous, P <= 0.015 %
<= 0.015 %
Silicon, Si <= 0.40 %
<= 0.40 %
Sulfur, S <= 0.0050 %
<= 0.0050 %