Tipco Tipcolene® FPDZ-1000 - 25% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FPDZ-1000 - 25% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Elongation at Break >= 80 %
>= 80 %
ASTM D638
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648