Tipco Tipcolene® SEB 300 M - 30% Chemically Coupled Glass Fibers & Mineral Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® SEB 300 M - 30% Chemically Coupled Glass Fibers & Mineral Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Mineral + Glass Reinforced, PP Homopolymer for Automobile Engine PartsApplications: Automotive Engine PartsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Break >= 8.0 %
>= 8.0 %
ASTM D638
Flexural Yield Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648