Tisan TISBLEND® PC/ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Tisan Engineering Plastics
Trade Name TISBLEND®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tisan TISBLEND® PC/ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High impact resistanceToughnessDimensional stabilityExcellent surface qualityHigh temperature enduranceEasy processability They have excellent chemical resistance to weak acids. They have good resistance to strong acids and weak alkalis. They have medium resistance to strong alkalis. They have weak resistance to organic solvents, alcohols, hydrocarbons, and engine fuels.
Thermal Properties Metric English Comments
Melting Point 220 - 270 °C
428 - 518 °F
Processing Properties Metric English Comments
Feed Temperature 70.0 °C
158 °F
Rear Barrel Temperature 220 - 230 °C
428 - 446 °F
Aft-1. Region Temperature
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Mid-2. Region Temperature
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Pre-3. Region Temperature
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Melt Temperature 220 - 270 °C
428 - 518 °F
Drying Temperature 90.0 - 120 °C
194 - 248 °F
Predrying Temperature
Dry Time 3 - 5 hour
3 - 5 hour
Predrying Time
Descriptive Properties Value Comments
Block Temperature 70°C