Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Tisan Engineering Plastics
Trade Name TISLAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tisan TISLAMID® 6 30% Glass Filled Impact Modified, Heat Stabilized Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElectric isolationEasy processabilityHigh mechanical resistanceExcellent flame retardanceHigh moisture absorptionExcellent temperature resistanceHigh performance / affordable priceAbrasion resistanceTISLAMID has an excellent resistance to weak alkalis and organic solvents. It has a good resistance to weak acids, alcohols, hydrocarbons, and engine fuels. It has a medium resistance to strong alkalis and a weak resistance to strong acids.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Ash 30 %
30 %
ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 99.0 MPa
14400 psi
ISO 527-2
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527-2
Elongation at Break 4.25 %
4.25 %
ISO 527-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-2
Modulus of Elasticity 6.30 GPa
914 ksi
ISO 527-2
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 205 °C
401 °F
ISO 306
Heat Distortion Temperature 215 °C
419 °F
ISO 75-2
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
60695-2-10
Electrical Properties Metric English Comments
Comparative Tracking Index 500 V
500 V
TS EN 60112
Processing Properties Metric English Comments
Feed Temperature 60.0 - 80.0 °C
140 - 176 °F
Rear Barrel Temperature 220 - 240 °C
428 - 464 °F
Aft-1. Region Temperature
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Mid-2. Region Temperature
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Pre-3. Region Temperature
Nozzle Temperature 210 - 230 °C
410 - 446 °F
Melt Temperature 220 - 240 °C
428 - 464 °F
Drying Temperature 90.0 - 100 °C
194 - 212 °F
Predrying Temperature
Dry Time 3 - 4 hour
3 - 4 hour
Predrying Time
Moisture Content 1.9 %
1.9 %
ISO 62
Descriptive Properties Value Comments
Block Temperature 60-80°C
Users viewing this material also viewed the following: