Toho Tenax Besfight® G40-800 24K IMA5C EP03 Continuous Filament Carbon Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Toho Tenax Co., Ltd.
Trade Name Besfight®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toho Tenax Besfight® G40-800 24K IMA5C EP03 Continuous Filament Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
Fiber Count 8400 dtex
7560 denier
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5580 MPa
810000 psi
Elongation at Break 1.95 %
1.95 %
Tensile Modulus 286 GPa
41500 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 0.00140 ohm-cm
0.00140 ohm-cm
Descriptive Properties Value Comments
Filament Diameter 5 µm
Size Level 1.3%
Users viewing this material also viewed the following: