Topas Advanced Polymers TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC)

Category Polymer , Thermoplastic , Cyclo Olefin Polymer
Manufacturer Topas Advanced Polymers
Trade Name TOPAS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Topas Advanced Polymers TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TOPAS® 6013M-07 is an injection molding grade with a wide processing window, especially suited for blow molding processes including IBM and ISBM. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface making it an excellent choice for healthcare and other high-tech products. Lower leachables and extractables of TOPAS COC preserve food and drug stability and quality. It is a non-polar substrate that does not promote adsorption, denaturation, aggregation, or precipitation like glass can. This grade has a high (130°C) heat distortion temperature to withstand 121°C steam sterilization protocols, as well as gamma and EtO procedures. Key applications and attributes: Drug delivery: Low leachables & extractables, low water transmission Prefilled syringes, vials, cartridges: Non-ionic, does not promote adsorption like glass Bottles: Minimally reactive, EtO/gamma/steam sterilizable Surgical instruments: Chemically resistant to alcohol, acetone, and acrylates IV containers and components: Transparent, withstands EtO/gamma/steam sterilization Labware: Temperature resistance, clarity and purity Optics: Clarity, low birefringence, low moisture sensitivity Electronics: Low dielectric constant, thermoplastic Healthcare and food: Broad regulatory approval Information provided by TOPAS Advanced Polymers
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption at Saturation 0.010 %

@Temperature 23.0 °C
0.010 %

@Temperature 73.4 °F
ISO 62
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 260 °C
12 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Stress 63.0 MPa
9140 psi
Break, (5mm/min); ISO 527-2,-1A
Elongation at Yield 2.6 %
2.6 %
5mm/min; ISO 527-2/1A
Tensile Modulus 2.90 GPa
421 ksi
1mm/min; ISO 527-2/1A
Charpy Impact Unnotched 1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.170 J/cm²

@Temperature 23.0 °C
0.809 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ISO 75-1,-2
Glass Transition Temp, Tg 142 °C
288 °F
10°C/min; ISO 11357-1,-2,-3
Optical Properties Metric English Comments
Refractive Index 1.53
1.53
ISO 489
Transmission, Visible 91 %
91 %
ISO 13468-2