Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total 50100.2 HDPE blow molding, sheet, thermoforming resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total 50100.2 HDPE blow molding, sheet, thermoforming resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging, sheet extrusion, thermoforming, truck bed liners, dunnage containers, large part formed articles. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt temperature 380 - 480ºF Thermoforming surface temperature 310 - 360 ºFInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 600 hour
>= 600 hour
ASTM D1693 cond. B 100% lgepal
High Load Melt Index 9.0 g/10 min

@Load 21.6 kg
9.0 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 26.2 MPa
>= 3800 psi
ASTM D 638 type IV
Elongation at Break 600 %
600 %
ASTM D 638, type IV
Flexural Modulus 1.210 GPa
175.5 ksi
ASTM D 790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Melting Point 127 °C
260 °F
ASTM D3417
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved