Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total CD 471 HDPE conduit

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Total Atofina
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total CD 471 HDPE conduit.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
ASTM D1693 cond. B 10% lgepal
>= 1000 hour
>= 1000 hour
ASTM D1693 cond. C 100% lgepal
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
High Load Melt Index 20 g/10 min

@Load 21.6 kg
20 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D 2240
Tensile Strength, Yield >= 22.8 MPa
>= 3300 psi
ASTM D 638 type IV
Elongation at Break >= 600 %
>= 600 %
ASTM D 638 type IV
Flexural Modulus 0.793 GPa
115 ksi
ASTM D 790
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Melting Point 126 °C
259 °F
ASTM D3417