Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 58 Shore A  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Styrene-Butadiene
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 58 Shore A  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides excellent mechanical and elastic properties to compound.Applications: Thanks to its high molecular weight Finaprene® 411x is designed for the compounding industry. This crumb shape, along with the high molecular weight confer a quick and important oil absorption capacity to the polymer and lead tot eh production of economical compounds while keeping good mechanical properties.Content of the compound for which the listed properties apply: F484: 72F435: 37F411X: 15Oil: 41GPPS: 20HIPS: 20CaCO3: 15Additional Notes: DIN Abrasion: 190 mm³Rossflex 100%: 43000 cyclesRossflex 300%: 80000 cyclesRossflex 500%: 112000 cyclesData provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Viscosity Measure 25 cSt
25 cSt
Toluene Solution; Finaprene 1008 Test
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 190 °C
29 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
Finaprene 1505 Test
Tensile Strength, Ultimate 5.10 MPa
740 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
unusually low elongation - error in manufacturer testing?; ASTM D638
Flex Crack Resistance 43000
43000
cycles per Rossflex 100%
80000
80000
cycles per Rossflex 300%
112000
112000
cycles per Rossflex 500%
Abrasion 190
190
mm³; DIN Abrasion