Total Finaprene® 507 Styrene-Butadiene TPE Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Styrene-Butadiene
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finaprene® 507 Styrene-Butadiene TPE Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene CopolymerDescription: Finaprene® 507 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high styrene content, Finaprene® 507 provides excellent mechanical properties to the compound along with a good fluidity.Applications: Thanks to its high fluidity Finaprene® 507 is designed for the compounding industry. Finaprene® 507 can be used as an alternative to GPPS to provide compounds hardness without imparting other compounds properties such as abrasion resistance or flexural resistance.Data provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Finaprene 2602 Test
Melt Flow 7.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
7.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
Finaprene 1505 Test
Tensile Strength, Ultimate 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Chemical Properties Metric English Comments
Styrene Content 27 %
27 %
Finaprene 1004 Test
Butadiene Content 73 %
73 %
Finaprene 1004 Test