Material Notes:
Finaprene® 602D is a clear high styrenic styrene-butadiene (SBS) block copolymer with a radial structure, which is widely used as modifiers or in alloys with many plastic resins, such polystyrene, polypropylene, polyethylene, polyester, etc. Especially the impact strength, the elongation and the flexibility of those plastic resins can be improved. Finaprene® 602D acts also as compatibilizer between various plastics, e.g. polyolefins and polystyrenes. The compatibilizing properties can therefore be used in recycling of mixed plastics waste.ApplicationIn blend with Finaclear® polymer and crystal polystyrene, Finaprene® 602D is used as additive to improve the impact strength of the blend while retaining good clarity.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895B
Density 0.960 g/cc
0.0347 lb/in³
Finaprene 2602 Method
Melt Index of Compound 8.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238G
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 MPa
2900 psi
ASTM D638
Elongation at Break <= 800 %
<= 800 %
ASTM D638
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Chemical Properties Metric English Comments
Styrene Content 40 %
40 %
Finaprene 1004 Method
Butadiene Content 60 %
60 %
Finaprene 1004 Method