Total Finathene® 6450 HDPE film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® 6450 HDPE film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D 792
Water Vapor Transmission 6.20 g/m²/day
0.399 g/100 in²/day
100°F; E 96/66
Thickness 25.4 microns
1.00 mil
Melt Flow 5.0 g/10 min

@Load 2.16 kg
5.0 g/10 min

@Load 4.76 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 850 %
850 %
ASTM D 882 A
Film Elongation at Break, TD 650 %
650 %
ASTM D 882
Secant Modulus, MD 0.689 GPa
99.9 ksi
ASTM D 882 A
Secant Modulus, TD 0.703 GPa
102 ksi
ASTM D 882 A
Film Tensile Strength at Break, MD >= 24.1 MPa
>= 3500 psi
ASTM D 882 A
Film Tensile Strength at Break, TD >= 26.2 MPa
>= 3800 psi
ASTM D 882 A
Thermal Properties Metric English Comments
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D 746
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ASTM D 1003
Gloss 75 %
75 %
ASTM D 523