Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total HDPE XT10 N High Density Polyethylene - Pipe Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Total Atofina
Trade Name HDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HDPE XT10 N High Density Polyethylene - Pipe Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyethylene: High molecular weight, bimodal pipe resin.Characteristics:Outstanding high temperature creep rupture strengthExceptional slow crack growth resistanceExcellent resistance to rapid crack growth propagationNSF certified to D2513 (gas), CSA B137.4 (gas), CSA B137.1 (water) and CSA C448 (geothermal)NSF Standard 14/61 CertifiedFDA CompliantApplications:Gas distributionPotable waterGeothermalIndustrial miningSewer and sewer reliningGas and oil gatheringGeneral pipe reliningPipe coatingInformation provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.949 g/cc
0.949 g/cc
ASTM D792
Melt Flow 7.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
PENT >= 5000 hour
>= 5000 hour
ASTM D1473
Tensile Strength, Yield >= 24.1 MPa
>= 3500 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 1.03 GPa

@Strain 2.00 %
150 ksi

@Strain 2.00 %
ASTM D790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Hydrostatic Design Basis 6.89 MPa

@Temperature 60.0 °C
1000 psi

@Temperature 140 °F
ASTM D2837
11.0 MPa

@Temperature 22.8 °C
1600 psi

@Temperature 73.0 °F
ASTM D2837
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
ASTM D3417
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Heat Distortion Temperature 77.8 °C
172 °F
ASTM D648
Brittleness Temperature -118 °C
-180 °F
ASTM D746
Descriptive Properties Value Comments
Cell Classification 445574, 445576
ASTM D3350
Minimum Required Strength 10 MPa
ISO 9080
Notched Pipe Test >500 hrs
ISO 13479
Pipe Test Category C3
ASTM D2239
Resistance to Rapid Crack Propagation >12 bar
ISO 13477, S4, Critical Pressure, 0°C
Copyright © lookpolymers.com All Rights Reserved