Material Notes:
Low density radical polyethylene made by high pressure autoclave process. Grade for very stiff and transparent thin film. Applications examples: rigid bags, automatic packaging, thin shrink film.. Advised temperature profile : 170 to 210°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D 792
Melt Flow 0.80 g/10 min
0.80 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.0 MPa
2030 psi
ISO R527
Tensile Strength, Yield 13.0 MPa
1890 psi
ISO R527
Elongation at Break 550 %
550 %
ISO R527
Modulus of Elasticity 0.350 GPa
50.8 ksi
ISO 5527
Dart Drop Test 150 g
0.331 lb
50µ; ISO 7765-1
Thermal Properties Metric English Comments
Melting Point 116 °C
241 °F
ISO 11357-3
Vicat Softening Point 106 °C
223 °F
ISO 306
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
50µ; ASTM D 1003
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.