Total Lacqtene® 2007 TN 61 HDPE pipe  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® 2007 TN 61 HDPE pipe  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACQTENE® 2007 TN 61 is a high density homopolymer polyethylene produced by the gas phase polymerization process.LACQTENE® 2007 TN 61 is best processed between 190 and 230°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
ISO 1183
Melt Flow 0.70 g/10 min

@Load 2.16 kg
0.70 g/10 min

@Load 4.76 lb
ISO 1133
2.8 g/10 min

@Load 5.00 kg
2.8 g/10 min

@Load 11.0 lb
ISO 1133
High Load Melt Index 47 g/10 min

@Load 21.6 kg
47 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868
Tensile Strength, Yield 29.0 MPa
4210 psi
ISO 527-2
Elongation at Break >= 700 %
>= 700 %
ISO 527-2
Flexural Modulus 1.55 GPa
225 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 136 °C
277 °F
ISO 3146
Vicat Softening Point 132 °C
270 °F
ISO 306
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.