Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lacqtene® FB 3010 LDPE blown film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® FB 3010 LDPE blown film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 180 to 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 0.27 g/10 min
0.27 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
ISO R527
Tensile Strength, Yield 11.0 MPa
1600 psi
ISO R527
Elongation at Break 650 %
650 %
ISO R527
Modulus of Elasticity 0.215 GPa
31.2 ksi
ISO 5527
Dart Drop Test 250 g
0.551 lb
50µ; ISO 7765-1
Thermal Properties Metric English Comments
Melting Point 112 °C
234 °F
ISO 11357-3
Vicat Softening Point 96.0 °C
205 °F
ISO 306
Optical Properties Metric English Comments
Haze 18 %
18 %
50µ; ASTM D 1003
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved