Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lumicene® mPE M5220 Metallocene High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Total Atofina
Trade Name Lumicene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® mPE M5220 Metallocene High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is a Total Ecosolutions grade.Lumicene® mPE M 5220 is a High Density Polyethylene with very good organoleptic properties, dimensional stability, stress-cracking resistance, rigidity and processability.It is especially suited for the production of beverage caps & closures by injection or compression molding, more specifically for carbonated drinks.This grade does not contain a slip agent.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133/D
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Tensile Modulus 1.00 GPa
145 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
ISO 11357
Processing Properties Metric English Comments
Melt Temperature <= 250 °C
<= 482 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved