Total MDPE 3802 B Medium Density Polyethylene, Pipes & Fittings

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Total Atofina
Trade Name MDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total MDPE 3802 B Medium Density Polyethylene, Pipes & Fittings.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MDPE 3802 B is a high performance hexene-based black compound, with a MRS 8 MPa - PE 80 classification, and primarily intended for potable water and gas pipe applications.MDPE 3802 B key characteristics are a superior resistance to slow crack growth ensuring safe and long-term network operation,an optimal balance of flexibility and mechanical strength that allows easy coiling, handling and installing of pipes,an optimized formulation of additives and finely dispersed carbon black providing outstanding long-term stability in service.Designation ISO 1872-PE,E/M-ACGHL,40-T012.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.948 g/cc
0.948 g/cc
ISO 1183
Carbon Black Loading 2.0 - 2.5 %
2.0 - 2.5 %
ISO 6964
Melt Flow 0.90 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.90 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133/T
Processing Properties Metric English Comments
Processing Temperature 190 - 220 °C
374 - 428 °F
Extrusion
200 - 260 °C
392 - 500 °F
Injection
Descriptive Properties Value Comments
Carbon Black Dispersion, Rating = 3
ISO 18553
Thermal Stability 200°C > 20 min
EN 728 / ISO 11357-6
Water Content = 300 ppm
EN 12118, measured at the stage of compound manufacturing