Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Total Atofina
Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization package.Polypropylene AUTOMOTIVE PPC 3060 MW5 has been especially developed for use in automotive applications.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-2
Tensile Modulus 1.30 GPa
189 ksi
ISO 527-2
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²

@Temperature -20.0 °C
2.62 ft-lb/in²

@Temperature -4.00 °F
ISO 180
10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
120°C per hour; ISO 752
Vicat Softening Point 65.0 °C

@Load 5.10 kg
149 °F

@Load 11.2 lb
50°C per hour; ISO 306
135 °C

@Load 1.02 kg
275 °F

@Load 2.25 lb
50°C per hour; ISO 306