Material Notes:
TOTAL Petrochemicals Polypropylene 4944CWZ is a nucleated and controlled rheology impact copolymer with a very high Melt Flow index of 50 g/10 min.TOTAL 4944CWZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent antistatic properties and mold release characteristics.Total Polypropylene 4944CWZ has been developed for high speed injection molding of thin-walled packaging containers and household articles.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 50 g/10 min
50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Pressure unspecified; ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525