Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina 3371 is available with custom slip and antiblock packages.FDA - Fina 3371 complies with all applicable FDA regulations and may be used under these provisions for food contact packaging.Recommended Applications - Fina 3371 is recommended in orientation processes for manufacture of packaging tapes and films.Processing - Fina 3371 resin processes on cast and oriented film extrusion equipment with typical melt temperatures of 450°F-525°F (232°C-274°C).Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Water Vapor Transmission 4.70 g/m²/day

@Temperature 37.8 °C
0.303 g/100 in²/day

@Temperature 100 °F
90% RH; thickness not specified; ASTM E96
Melt Flow 2.8 g/10 min
2.8 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 130 %
130 %
ASTM D882
Film Elongation at Break, TD 50 %
50 %
ASTM D882
Secant Modulus, MD 2.41 GPa
350 ksi
ASTM D882
Secant Modulus, TD 4.14 GPa
600 ksi
ASTM D882
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
Film Tensile Strength at Break, TD 262 MPa
38000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
DSC
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Gloss 90 %
90 %
45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 232 - 274 °C
450 - 525 °F
oriented film extrusion