Material Notes:
Polypropylene 3576 H is recommended for use core layer in non-oriented cast films processes for the manufacture of packaging film with outstanding optical properties. 3576 H is specially designed for metalizable films.3576 H is intended for food, magazine or textile packaging, for lamination films as well as for stationary supplies.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Vicat Softening Point 152 °C

@Load 1.02 kg
306 °F

@Load 2.25 lb
ASTM D1525
Descriptive Properties Value Comments
Isotacticity Index (%) 97.5
Total Internal Test