Material Notes:
ATOFINA Polypropylene PPH 9059 is homopolymer.ApplicationATOFINA Polypropylene PPH 9059 is intended for extrusion of bulk continuous filament (BCF) and continuous filament (CF) fibers. PPH 9059 has a special anti gas-fading formulation to significantly reduce yellowing in fibers.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ISO 2039-2
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527-2
Elongation at Yield 9.0 %
9.0 %
ISO 527-2
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-2
Flexural Modulus 1.50 GPa
218 ksi
ISO 527-2
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
120°C per hour; ISO 75-2
Vicat Softening Point 89.0 °C
192 °F
50N-50°C per hour; ISO 306
153 °C
307 °F
10N-50°C per hour; ISO 306