Material Notes:
Total Petrochemicals PPR 12232 is a high melt flow index, high transparency random copolymer. Its has an excellent food compatibility due to its low odor, making it especially suitable for the production of food packaging and housewares products. Its high fluidity accounts for significant cycle time reduction.Peroxide is not used in the manufacturing of the above mentioned product.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ISO 2039-2
Flexural Modulus 1.15 GPa
167 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 67.0 °C

@Load 5.10 kg
153 °F

@Load 11.2 lb
50°C per hour; ISO 306
130 °C

@Load 1.02 kg
266 °F

@Load 2.25 lb
50°C per hour; ISO 306