Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color/Clarity/Impact. TOTAL Petrochemicals Polypropylene Z9421 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable. The very low melting point of Z9421 makes it an excellent heat seal layer for oriented films.FDA. Z9421 complies with all applicable FDA regulations Title 21 CFR Section 177.1520(c) 3.1 and may be used under these provisions for food contact and packaging.Recommended Applications. Z9421 is recommended for use in non-oriented film processes for manufacture of films that require improved optical and impact properties and as a heat seal layer for oriented films.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D1505
Water Vapor Transmission 18.6 g/m²/day

@Temperature 37.8 °C
1.20 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249-90
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.7 MPa
3000 psi
non-oriented film; ASTM D882
Elongation at Break 350 %
350 %
ASTM D882
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Thermal Properties Metric English Comments
Melting Point 120 °C
248 °F
DSC
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 80 %
80 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 193 - 227 °C
379 - 441 °F
Users viewing this material also viewed the following: