Total PSC 1050 High Heat Resistance, High Molecular Weight Crystal Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Heat Resistant Grade
Manufacturer Total Atofina
Trade Name PSC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSC 1050 High Heat Resistance, High Molecular Weight Crystal Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Total Petrochemicals Polystyrene 1050 is a high heat resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, where it yields expanded sheets with high mechanical properties. Polystyrene Crystal 1050 can be used in dilution with HIPS for the extrusion of sheet for hot-fill thermoforming applications. Polystyrene Crystal 1050 does contain external lubrication.Suitable applications for Total Petrochemicals Polystyrene 1050 include foamed trays, shower screens and high heat thermoformed products.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Water Absorption 0.040 %
0.040 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 70
70
ASTM D785
Tensile Strength at Break 53.0 MPa
7690 psi
ASTM D638
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 89.0 µm/m-°C
49.4 µin/in-°F
ASTM D696
Vicat Softening Point 108 °C

@Load 1.02 kg
226 °F

@Load 2.25 lb
50°C per hour; ASTM D1525
Heat Distortion Temperature 92.2 °C
198 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC 93
Dielectric Strength 152 kV/mm
3860 kV/in
ASTM D149