Toyobo A1064D Thermoplastic Polyurethane Elastomer, Injection Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Toyobo
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo A1064D Thermoplastic Polyurethane Elastomer, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Ultimate 47.0 MPa
6820 psi
ASTM D638
Tensile Strength, Yield 22.6 MPa

@Strain 100 %
3280 psi

@Strain 100 %
ASTM D638
Elongation at Break 440 %
440 %
ASTM D638
Tear Strength 245 kN/m
1400 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 75
75
H22
Compression Set 40 %
40 %
ASTM D395B
Thermal Properties Metric English Comments
Vicat Softening Point 137 °C
279 °F
ASTM D1525
Brittleness Temperature <= -65.0 °C
<= -85.0 °F
ASTM D746