Toyobo A2080A Thermoplastic Polyurethane Elastomer, Injection Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Toyobo
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo A2080A Thermoplastic Polyurethane Elastomer, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength, Ultimate 34.0 MPa
4930 psi
ASTM D638
Tensile Strength, Yield 5.40 MPa

@Strain 100 %
783 psi

@Strain 100 %
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Tear Strength 93.0 kN/m
531 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 20
20
H22
Compression Set 35 %
35 %
ASTM D395B
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746