Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Toyobo
Trade Name VYLOPET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemical & weather resistance, and processability.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength, Ultimate 147 MPa
21300 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Flexural Modulus 9.10 GPa
1320 ksi
ASTM D790
Compressive Yield Strength 108 MPa
15700 psi
ASTM D695
Izod Impact, Notched 1.80 J/cm
3.37 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 15
15
ASTM D1044
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
UL RTI, Electrical 130 °C
266 °F
UL-746B
Flammability, UL94 HB

@Thickness 0.7937 mm
HB

@Thickness 0.03125 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 25.0 kV/mm

@Thickness 2.00 mm
635 kV/in

@Thickness 0.0787 in
ASTM D149
Arc Resistance 130 sec
130 sec
ASTM D495
Comparative Tracking Index 255 V
255 V
IEC test
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved