Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, ceramics, most plastics and metals, and is particularly recommended for applications where dependable, reputable performance is required, including assembly and repair of fiber optic connectors, high performance electronic and aerospace systems, medical device assembly, and for structural laminating applications. The fully cured TRA-BOND 2105 is a good electrical insulator, has a high glass transition temperature for good rigidity and provides excellent resistance to weather, galvanic action, salt solutions and many chemicals including mild acids and alkalis, petroleum solvents, lubricating oils, jet fuels, gasoline and alcohol. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Volatile Organic Compounds (VOC) Content 3.52 g/l
3.52 g/l
Water Absorption 0.24 %
0.24 %
After 24 hours
Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
1 hr @ 65°C
Elongation at Yield 4.0 %
4.0 %
Adhesive Bond Strength 15.9 MPa
2300 psi
Lap shear, alum to alum, 1 hr @ 65°C
19.3 MPa
2800 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 140 °C
284 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 120 °C
248 °F
Ultimate Tg
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Constant 4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm
420 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 20 min
20 min
Descriptive Properties Value Comments
Color Clear
Cytotoxicity Study Passes
ISO 10993-5, elution method
Mix Ratio, parts by weight 100/25
Resin/Hardener
Thixotropic Index 1