Material Notes:
TRA-CAST 216H02 is a medium viscosity two-part formulation recommended for general purpose electrical potting and encapsulation applications where the combination of good mechanical thermal and electrical properties are required. It is opaque in coating applications when the applied thickness exceeds 0.2mm. It is an all liquid system with excellent flow and wetting characteristics, exhibits superior adhesion to glass, ceramics, most metals, many plastics (includes potting shells) and other electronic materials, contains no solvents and is easily mixed, handled and cured with minimum shrinkage at room temperatures. The fully cured TRA-CAST 216H02 is an electrical insulator with good impact and thermal shock resistance. It is further resistant to water, weather, gases, galvanic action, petroleum fuels and solvents, alcohol, salts and many acids and alkalis. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 12000 cP

@Temperature 25.0 °C
12000 cP

@Temperature 77.0 °F
Mixed (sp #7, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
24 hrs @ 25°C
Adhesive Bond Strength 7.58 MPa
1100 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 75.0 °C
167 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 17 min
17 min
35 grams
Descriptive Properties Value Comments
Color Black
Resin/Mixed/Cured
Light Yellow
Hardener
Working Life minutes 50
35 grams