Tra-Con Tra-Bond 724-9 Polyurethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 724-9 Polyurethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 724-9 premixed and frozen polyurethane adhesive has excellent adhesion and provides strong resilient bonds to a wide variety of substrates including aluminum, solder, nylon, mylar and steel.Information provided by Tra-Con Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
Adhesive Bond Strength 7.93 MPa
1150 psi
Lap shear, alum to alum
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 75.0 °C
3.00 hour

@Temperature 167 °F
Descriptive Properties Value Comments
Color Amber
Users viewing this material also viewed the following: