Tra-Con Tra-Bond FDA16 Food and Drug Application Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FDA16 Food and Drug Application Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FDA-16 EPOXY ADHESIVE is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received Class VI approval. This two-part amber adhesive is commonly used for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND FDA-16 EPOXY ADHESIVE is an effective electrical insulator, and it provides low permeability to gases and vapors, and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds. Though not fully cured, significant properties develop after 24 hours @ 25°C.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Volatile Organic Compounds (VOC) Content 0.15 g/l
0.15 g/l
Water Absorption 0.30 %
0.30 %
After 24 hours
Viscosity 4700 cP

@Temperature 25.0 °C
4700 cP

@Temperature 77.0 °F
Mixed (sp #4, 12 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
24 hrs @ 25°C
86
86
4 hrs @ 65°C
Adhesive Bond Strength 13.8 MPa
2000 psi
Lap shear, alum to alum, 24 hrs @ 25°C
23.4 MPa
3400 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 20.0 °C
29.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 145 °C
293 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 97.0 °C
207 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+14 ohm-cm
1.20e+14 ohm-cm
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Pot Life 25 min
25 min
25 grams
Descriptive Properties Value Comments
Color Amber
Mix Ratio, parts by weight 100/33
Resin/Hardener