Tra-Con Tra-Bond FS411 Fast Cure Epoxy Adhesive System

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FS411 Fast Cure Epoxy Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FS-411 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. It was designed to have low outgassing in vacuum applications. This versatile two-part epoxy system contains no solvents, mixes easily at room temperature, and is suitable for high performance structural bonding applications. It develops strong, tough bonds to metals, plastics, glass and glass fabrics, hardboards and forestry products, ceramics, rubber, masonry materials, and other construction materials. When fully cured, TRA-BOND FS- 411 is an excellent electrical insulator, and provides superior moisture resistance. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Cured
Viscosity 14000 cP
14000 cP
Hardener
430000 cP
430000 cP
Resin
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
2 hrs @ 65°C
80
80
24 hrs @ 25°C
Adhesive Bond Strength 28.3 MPa
4100 psi
Lap shear, alum to alum, 24 hrs @ 25°C
31.0 MPa
4500 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 30.0 °C
86.0 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 10 min
10 min
Descriptive Properties Value Comments
Color Milky, Translucent