Tra-Con Tra-Cast 3101 Encapsulating Adhesive System

Category Polymer , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Cast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Cast 3101 Encapsulating Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-CAST 3101 is an easy-to-use, room temperature cure, rigid, low viscosity, 100% solids (no solvents) epoxy resin and hardener system with excellent mechanical and electrical properties. It is recommended for structural and electronic casting and encapsulating applications that require its excellent wetting and fluidity, good thermal expansion coefficients, and improved thermal shock resistance properties. TRA-CAST 3101 is readily mixed, handled and cured at room temperature, and it adheres to a wide range of materials including most metals, glass, ceramics and many plastics. Fully cured TRA-CAST 3101 is a strong, tough, durable electrical insulator which is also highly resistant to weather, water, gases and vapors, petroleum lubricants and fuels and many mild acids and alkalis.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Mixed
Viscosity 3000 cP

@Temperature 25.0 °C
3000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+14 ohm-cm
1.40e+14 ohm-cm
8.50e+10 ohm-cm

@Temperature 100 °C
8.50e+10 ohm-cm

@Temperature 212 °F
Dielectric Constant 3.9

@Frequency 1e+6 Hz
3.9

@Frequency 1e+6 Hz
4.2

@Frequency 1000 Hz
4.2

@Frequency 1000 Hz
Dielectric Strength 16.7 kV/mm
425 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
4 hrs @ 25°C + 2 hrs @ 65°C
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Tan
Heat Distortion Temperature °C 85
Mix Ratio, parts by weight 100/125
Resin/Hardener