Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-DUCT 925M01 is a low ion snap cure silver-filled epoxy. TRA-DUCT 925M01 develops strong, durable, void free electrically and thermally conducting bonds. The product can be screen printed, stenciled or applied with an automated high speed dot dispenser.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Cured
Viscosity 2500 cP
2500 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
Adhesive Bond Strength 10.3 MPa
1500 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C
17.2 µin/in-°F
Below Tg
120 µm/m-°C
66.7 µin/in-°F
Above Tg
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Volume Resistivity 0.00040 ohm-cm
0.00040 ohm-cm
Processing Properties Metric English Comments
Cure Time 1.00 min

@Temperature 175 °C
0.0167 hour

@Temperature 347 °F
5.00 min

@Temperature 150 °C
0.0833 hour

@Temperature 302 °F
15.0 min

@Temperature 120 °C
0.250 hour

@Temperature 248 °F
90.0 min

@Temperature 80.0 °C
1.50 hour

@Temperature 176 °F
720 min

@Temperature 50.0 °C
12.0 hour

@Temperature 122 °F
Pot Life 4320 - 5760 min
4320 - 5760 min
(3-4 days)
Descriptive Properties Value Comments
Color Silver