Trelleborg Emerson & Cuming EP578 Adhesive

Category Polymer , Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming EP578 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Density matched blue adhesive for use with EP678, TB610 and TB620.All information provided by Trelleborg Emerson & Cuming
Physical Properties Metric English Comments
Specific Gravity 0.650 g/cc
0.650 g/cc
ASTM D792
Viscosity 10000 cP

@Temperature 25.0 °C
10000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Thermal Properties Metric English Comments
CTE, linear 324 µm/m-°C
180 µin/in-°F
Processing Properties Metric English Comments
Pot Life 75 min

@Temperature 25.0 °C
75 min

@Temperature 77.0 °F
Gel Time 240 min

@Temperature 25.0 °C
240 min

@Temperature 77.0 °F
Thin Film
Descriptive Properties Value Comments
Color Blue