Trelleborg Emerson & Cuming Eccobond® 24 Two-Component High Strength-Impact Resistant Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 24 Two-Component High Strength-Impact Resistant Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 24 Eccobond® Two-Component High Strength-Impact Resistant Epoxy AdhesiveClear, low viscosity, room temperature curing, epoxy adhesive. Exhibits resilient bonds when joining dissimilar materials. Excellent impact resistance. Recommended for bonding glass, polystyrene, polysulfone, polycarbonate, rigid PVC and PVDC. Mix ratio of 100:28. Cure Type: Room Temp or Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Viscosity 800 cP

@Temperature 25.0 °C
800 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Adhesive Bond Strength 12.4 MPa
1800 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
240 min

@Temperature 45.0 °C
4.00 hour

@Temperature 113 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Clear