Trelleborg Emerson & Cuming Eccobond® 930-09 Low Temperature Performance Lighting Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 930-09 Low Temperature Performance Lighting Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 930-09 Eccobond® Low Temperature Performance Lighting Epoxy AdhesiveFlexible, non-blushing, epoxy adhesive for glass headlamp bonding. Maintains flexibility at temperatures as low as -40°C. Low volatility. Excellent humidity resistance. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.27 MPa
1200 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 160 °C
0.333 hour

@Temperature 320 °F
42.0 min

@Temperature 140 °C
0.700 hour

@Temperature 284 °F
Descriptive Properties Value Comments
Color Grey
Viscosity Thixotropic Paste