Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conductivity. Typical applications include a wide range of electrical components such as capacitors and transformers.Emerson & Cuming 2057FR/11 Stycast® Two-Component Epoxy Flame Retardant EncapsulantLow ViscosityGood Chemical ResistanceFilledHigh TemperatureMix Ratio by Weight = 100:8 Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
Viscosity 3400 cP
3400 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Thermal Properties Metric English Comments
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 155 °C
311 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 43.0 °C
109 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.4

@Frequency 1e+6 Hz
4.4

@Frequency 1e+6 Hz
Dielectric Strength 16.7 kV/mm
425 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min
0.500 - 1.00 hour