Trelleborg Emerson & Cuming Stycast® 2754 Two-Component Epoxy Flexible Low-Stress Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced , Epoxy, Thermally Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 2754 Two-Component Epoxy Flexible Low-Stress Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 2754 Stycast® Two-Component Epoxy Flexible Low-Stress EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components where shock and impact resistance are required. Typical applications include transformers, motors, coils, and other electrical devicesFeaturesThermally ConductiveGood Chemical ResistanceFilledMix Ratio (by weight) = 100:40 Cure Type: Room Temp or Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
Viscosity 24000 cP

@Temperature 25.0 °C
24000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Thermal Properties Metric English Comments
Thermal Conductivity 0.630 W/m-K
4.37 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.9

@Frequency 1e+6 Hz
4.9

@Frequency 1e+6 Hz
Dielectric Strength 17.7 kV/mm
450 kV/in
Processing Properties Metric English Comments
Cure Time >= 120 min
>= 2.00 hour