Trelleborg Emerson & Cuming Stycast® E-151-8 One-Component Epoxy Flexible Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® E-151-8 One-Component Epoxy Flexible Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming E-151-8 Stycast® One-Component Epoxy Flexible EncapsulantExcellent thermal shock and impact resistance. Good chemical resistance, high temperature, unfilled, low viscosity. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 1100 cP

@Temperature 25.0 °C
1100 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.4

@Frequency 1e+6 Hz
3.4

@Frequency 1e+6 Hz
Dielectric Strength 12.8 kV/mm
325 kV/in
Processing Properties Metric English Comments
Cure Time >= 15.0 min
>= 0.250 hour