Trimay® Wear Plate TWP61 Complex-carbide Flux Cored Weld Wire & Electrode

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Trimay® Wear Plate Ltd
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trimay® Wear Plate TWP61 Complex-carbide Flux Cored Weld Wire & Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TWP61 is a complex-carbide flux cored wire electrode used to protect equipment and parts from heavy wear in extreme temperatures. TWP61 has a unique composition that forms a tight crystalline matrix, and is able to deter heavy wear in temperatures up to 842oF (450oC).Key Performance Characteristics: Heavy abrasion resistance, High heat resistance, Tight crystalline matrix,Good corrosion resistance Applications: TWP61 can be overlain on carbon steel, manganese base materials and mild or alloy steels. The maximum recommended deposit thickness of TWP61 3/8” (9.53mm) in 2 - 3 layers. TWP61 is used for the installation of T157 wear plate and parts, as well as for hot wear applications such as burner tips, classifier cones and smokestacks.Information provided by Trimay®
Mechanical Properties Metric English Comments
Hardness, Rockwell C 60 - 64
60 - 64
Electrodes
63 - 65
63 - 65
Wire
Component Elements Properties Metric English Comments
Boron, B <= 1.5 %
<= 1.5 %
Carbon, C <= 5.0 %
<= 5.0 %
Chromium, Cr <= 30 %
<= 30 %
Iron, Fe <= 30 %
<= 30 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Tungsten, W <= 1.5 %
<= 1.5 %
Vanadium, V <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Available Sizes: Electrode 3.25
[mm]
4
[mm]
5
[mm]
Available Sizes: Wire 1.1
[mm], cored wire
1.6
[mm], cored wire
2.4
[mm], cored wire
2.8
[mm], cored wire
Packaging: Electrode 3.25
[mm] 4.5kg sleeves (4 sleeves=1 box)
4
[mm] 5kg sleeves (4 sleeves=1 box)
5
[mm] 5kg sleeves (4 sleeves=1 box)
Packaging: Wire 1.1
[mm], 15kg spools
1.6
[mm], 25kg spools
2.4
[mm], 25kg spools
2.8
[mm], 25kg spools