Material Notes:
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication Systems through the world.Comments: no plasticized, flexible materialInformation provided by UBE.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Melt Flow 14 g/10 min

@Load 1.00 kg,
Temperature 190 °C
14 g/10 min

@Load 2.20 lb,
Temperature 374 °F
ASTM D1238R
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength at Break >= 19.0 MPa
>= 2760 psi
ASTM D638
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Strength 7.00 MPa
1020 psi
ASTM D790
Flexural Modulus 0.150 GPa
21.8 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 154 °C
309 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648